ID |
Date |
Author |
Target Material |
Target Oven W.O# |
Source |
Status |
Subject |
Text |
 |
49
|
Wednesday, September 26, 2012, 15:14 |
Nikita Bernier | BeO | | | Done | Sintering BeO Pellets #4 | Wednesday, September 26, 2012, 15:07
|
|
48
|
Wednesday, September 26, 2012, 15:06 |
Nikita Bernier | TaC | | | Done | Sintering Ta foil with TaC coating |
|
 |
47
|
Monday, September 24, 2012, 18:09 |
Nikita Bernier | TaC | | | Done | Sintering Ta foil with TaC coating |
|
  |
46
|
Monday, September 24, 2012, 15:12 |
Nikita Bernier | TaC | | | Done | Sintering Ta foil with TaC coating | Monday, September 24, 2012, 15:01
The target boat with TaC coating
is being used again. The inside of the boat |
|
45
|
Wednesday, August 22, 2012, 17:36 |
John Wong | Empty | 39165-5 | LP-SIS | Done | Coating target oven /w TaC & sintering for UCx#5 | Wednesday, August 22, 2012, 17:25
Note: LP-FEBIAD target container
( W.O#37918-3) was coated with TaC and sintered |
|
44
|
Tuesday, August 14, 2012, 17:11 |
John Wong | | | | Failed | Sintering Ta2O5 coating on Ta foil failed |
|
|
43
|
Tuesday, August 14, 2012, 15:57 |
John Wong | SiC | 38295-8 | HP-FEBIAD | Done | Testing endcaps inserted /w the new expansion tool | Tuesday, August 14, 2012, 15:44
This SiC target was prepared in May
2011 with the Evaporator#1. The target |
 |
42
|
Tuesday, August 14, 2012, 15:11 |
John Wong | | | | Maintenance | Replacing Cu-heatshield insulators | Tuesday, August 14, 2012, 15:01
The Cu-heatshield insulators are
broken due to prolong heating time during |
 |
41
|
Monday, August 13, 2012, 13:50 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
|
40
|
Saturday, August 11, 2012, 19:21 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
 |
39
|
Friday, August 10, 2012, 19:57 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating | Friday, August 10, 2012, 19:54
|
|
38
|
Monday, July 30, 2012, 15:42 |
John Wong | | | | Problems | Chiller maybe leaky | Monday, July 30, 2012, 15:38
The evaporator was used for the processing
the NiO target for 8 days and it was discovered |
|
37
|
Sunday, July 22, 2012, 20:51 |
John Wong | NiO | 38481-7 | HP-FEBIAD | Done | Sintering NiO#1 | Sunday, July 22, 2012, 20:30
The NiO target materials were loaded
into the container today. |
   |
36
|
Thursday, July 19, 2012, 17:05 |
John Wong | Empty | 37918-3 | LP-FEBIAD | Done | Coating target oven /w TaC & sintering for UCx#5 | Thursday, July 19, 2012, 16:58
The target container was coated with
TaC. |
|
35
|
Tuesday, July 17, 2012, 16:00 |
John Wong | | targetboat (TaC coated) | | Done | Sintering TaC coated regular- & D-endcaps | Tuesday, July 17, 2012, 15:45
Target boat is filled with TaC coated
regular- and D-endcaps. |
|
34
|
Thursday, July 12, 2012, 17:55 |
John Wong | NiO | targetboat (TaC coated) | | Maintenance | NiO development- test#2 | Thursday, July 12, 2012, 17:29
NiO was sprayed on Ni foil.
Average/discs: mass= 0.075g, thickness=0.076mm, |
 |
33
|
Thursday, June 21, 2012, 18:13 |
John Wong | NiO | Ta target boat | | Failed | NiO development - Container broke! |
|
    |
32
|
Wednesday, June 20, 2012, 22:33 |
John Wong | NiO | Ta target boat | | Done | NiO development |
|
|
31
|
Wednesday, June 20, 2012, 17:29 |
Nikita Bernier | NiO | Ta target boat | | Done | NiO development | Wednesday, June 20, 2012, 17:23
New Target boat, with no coating,
wrapped with a 0.002 inches thick Ta foil, |
 |
30
|
Monday, June 11, 2012, 12:26 |
John Wong | SiC | 38481-2 | HP-SIS | Problems | End caps vaporized |
|
|