Entry  Friday, August 10, 2012, 19:57, Nikita Bernier, , , , Done, Sintering Ta foil with TaO coating 
    Reply  Saturday, August 11, 2012, 19:21, Nikita Bernier, , , , Done, Sintering Ta foil with TaO coating TaO1.pngTaO2.png
       Reply  Monday, August 13, 2012, 13:50, Nikita Bernier, , , , Done, Sintering Ta foil with TaO coating TaO3.png
          Reply  Tuesday, August 14, 2012, 17:11, John Wong, , , , Failed, Sintering Ta2O5 coating on Ta foil failed Ta2O5_coating.PNG
Message ID: 39     Entry time: Friday, August 10, 2012, 19:57     Reply to this: 40
Author: Nikita Bernier 
Target Material:  
Target Oven W.O#:  
Source:  
Status: Done 
Subject: Sintering Ta foil with TaO coating 

 Friday, August 10, 2012, 19:54

 

Target boat with TaC coating, inside covered with a 0.002 inches thick Ta foil, wrapped with a 0.002 inches thick Ta foil, contains a Ta foil with TaO coating.

See John's Ipad for their recipes.

Evaporator #2 is now auto-ramping overnight at 0.2 A/min, up to 830 A, with the maximum voltage limited at 14 V, between 2.00e-05 (Good vacuum) and 3.00e-05 Torr (Bad vacuum).

 