21
|
Wednesday, May 16, 2012, 14:04 |
John Wong | | | | Problems resolved | TBHT cooling line leaky |
|
|
|
28
|
Monday, May 28, 2012, 11:15 |
John Wong | | | | Problems | Chiller is leaking water | Monday, May 28, 2012, 11:08
It was discovered this morning that
the Evaporator #2 chiller was leaking water |
|
|
35
|
Tuesday, July 17, 2012, 16:00 |
John Wong | | targetboat (TaC coated) | | Done | Sintering TaC coated regular- & D-endcaps | Tuesday, July 17, 2012, 15:45
Target boat is filled with TaC coated
regular- and D-endcaps. |
|
|
38
|
Monday, July 30, 2012, 15:42 |
John Wong | | | | Problems | Chiller maybe leaky | Monday, July 30, 2012, 15:38
The evaporator was used for the processing
the NiO target for 8 days and it was discovered |
|
|
39
|
Friday, August 10, 2012, 19:57 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating | Friday, August 10, 2012, 19:54
|
|
|
40
|
Saturday, August 11, 2012, 19:21 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
|
|
41
|
Monday, August 13, 2012, 13:50 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
|
|
42
|
Tuesday, August 14, 2012, 15:11 |
John Wong | | | | Maintenance | Replacing Cu-heatshield insulators | Tuesday, August 14, 2012, 15:01
The Cu-heatshield insulators are
broken due to prolong heating time during |
|
|
44
|
Tuesday, August 14, 2012, 17:11 |
John Wong | | | | Failed | Sintering Ta2O5 coating on Ta foil failed |
|
|
|
53
|
Friday, January 11, 2013, 11:16 |
John Wong | | | | Maintenance | Replace terminal insulator | Friday, January 11, 2013, 10:59
The insulator that holds the terminals
was broken when a target container was installed. |
|
|
55
|
Friday, January 11, 2013, 15:16 |
Anders Mjos | | | | Maintenance | Replace terminal insulator |
|
|
|
56
|
Tuesday, January 22, 2013, 16:14 |
John Wong | | | LP-SIS | Done | Heating RFQ components & measuring temperatures | Tuesday, January 22, 2013, 12:38
This is to test the newly developed
RFQ target to be commissioned this year. |
|
|
76
|
Tuesday, May 28, 2013, 17:50 |
John Wong | | Target Boat #2 | | Done | Sintering TaC coated end caps | Tuesday, May 28, 2013, 17:36
The target containers endcaps were
coated with TaC solution and let dry. |
|
|
83
|
Tuesday, August 27, 2013, 17:01 |
John Wong | | targetboat (TaC coated) | | Done | Sintering TaC coated regular caps | Tuesday, August 27, 2013, 16:48
Target boat is filled with TaC coated
endcaps (brown) and some partial sinterred |
|
|
84
|
Thursday, August 29, 2013, 11:53 |
Laura Lambert | | targetboat (TaC coated) | | Done | Sintering TaC coated regular caps |
|
|
|
92
|
Tuesday, October 29, 2013, 15:50 |
Anders Mjos | | | | In progress | Copper bars on TGHT and TBHT | Tuesday, October 29, 2013, 15:50:
Pumping down
Wednesday, October 30, 2013, 09:32: |
|
|
93
|
Friday, November 01, 2013, 17:20 |
Anders Mjos | | | | Problems | Backing pump needs new filter | The source of the poor vacuum in the backing
line seems to be related to a dirty filter.
We will try to find a replacement filter |
|
|
94
|
Monday, November 04, 2013, 14:02 |
Anders Mjos | | | | Maintenance | Backing pump replaced |
|
|
|
96
|
Thursday, November 07, 2013, 09:38 |
Anders Mjos | | | | Problems resolved | Heat Shield cooling line twisted | See attached photo.
The Heat Shield has been taken to
the Machine Shop for repair. |
|
|
115
|
Tuesday, January 28, 2014, 15:46 |
Laura Lambert | | 40282-4 | TARGET BOAT | Failed | Sintering TaC coated end caps | Tuesday, January 28, 2014, 15:43
The target containers end-caps were
coated with TaC spray and let dry. |
|