Friday, January 31, 2014, 12:10, Laura Lambert, Empty, 39165-10, LP-SIS, Done, Sintering TaC coating container for Ta?
|
Friday, January 31, 2014, 11:28
Target container is coated with TaC.
The container is wrapped with 3 x Ta heat-shield. |
Thursday, April 09, 2015, 09:38, Laura Lambert, Empty, 38817-7, HP-SIS, Done, Sintering TaC coating container for SiC#32
|
Thursday, April 09, 2015, 09:33
Target container is coated with TaC and wrapped with 3-Ta heat shields, not incl center block.
TGHT and TBHT will be ramped up to 820A and 230A, respectively. |
Tuesday, June 17, 2014, 13:20, Laura Lambert, Empty, 39530-8, HP-FEBIAD, Done, Sintering TaC coating container for SiC#30 part 2
|
Tuesday, June 17, 2014, 13:11
Target container is coated with TaC.
Container is wrapped with 3x Ta-heat shields. |
Wednesday, September 07, 2016, 15:02, John Wong, Empty, 39530-9, HP-SIS, In progress, Sintering TaC coating container for SiC Target  
|
Wednesday, September 07, 2016, 14:45
Container was previously coated with TaC solution and wrapped with 1-full length layer of Ta- heat shield around the fins.
Chamber is being pumped down. Vac at 5.6e-7 Torr before HS water valves were open; no leaks were detected. |
Tuesday, August 25, 2015, 11:54, Laura Lambert, Empty, , HP-FEBIAD, In progress, Sintering TaC coating container for SiC Target
|
Tuesday, August 25, 2015, 11:50
Container coated with TaC using new method: Ends tapped off, with liquid poured in and swirled around entire container, then poured back
out - 'flushing technique' |
Thursday, August 27, 2015, 16:37, John Wong, Empty, , HP-FEBIAD, Done, Sintering TaC coating container for SiC Target
|
Laura Lambert wrote:
Tuesday, August 25, 2015, 11:50 |
Thursday, January 16, 2014, 13:06, Laura Lambert, Empty, 39165-9, LP-SIS, In progress, Sintering TaC coating container
|
John Wong wrote:
Wednesday, January 15, 2014, 17:30 |
Friday, January 17, 2014, 09:34, John Wong, Empty, 39165-9, LP-SIS, In progress, Sintering TaC coating container
|
Laura Lambert wrote:
|
Friday, January 17, 2014, 12:52, John Wong, Empty, 39165-9, LP-SIS, In progress, Sintering TaC coating container
|
Laura Lambert wrote:
|
Monday, January 20, 2014, 16:30, Laura Lambert, Empty, 39165-9, LP-SIS, Done, Sintering TaC coating container
|
John Wong wrote:
|
Wednesday, January 15, 2014, 17:45, John Wong, Empty, 39165-9, LP-SIS, In progress, Sintering TaC coating container
|
Wednesday, January 15, 2014, 17:30
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Friday, January 17, 2014, 10:18, Laura Lambert, Empty, 39165-9, LP-SIS, In progress, Sintering TaC coating container
|
John Wong wrote:
|
Monday, June 29, 2015, 16:18, Laura Lambert, Empty, 41369-2, LP-SIS, In progress, Sintering TaC coating container
|
Monday, June 29, 2015, 16:17
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Monday, June 29, 2015, 23:42, John Wong, Empty, 41369-2, LP-SIS, In progress, Sintering TaC coating container
|
Laura Lambert wrote:
Monday, June 29, 2015, 16:17 |
Tuesday, June 30, 2015, 09:50, Laura Lambert, Empty, 41369-2, LP-SIS, In progress, Sintering TaC coating container   
|
John Wong wrote:
|
Monday, July 06, 2015, 12:07, John Wong, Empty, 41369-2, LP-SIS, In progress, Sintering TaC coating container
|
Laura Lambert wrote:
|
Monday, July 06, 2015, 16:30, Laura Lambert, Empty, 41369-2, LP-SIS, Done, Sintering TaC coating container   
|
John Wong wrote:
|
Wednesday, July 23, 2014, 15:07, John Wong, Empty, 40282-3, LP-SIS, In progress, Sintering TaC coated target container
|
Wednesday, July 23, 2014, 15:07
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Monday, July 28, 2014, 10:52, Laura Lambert, Empty, 40282-3, LP-SIS, Done, Sintering TaC coated target container
|
John Wong wrote:
Wednesday, July 23, 2014, 15:07 |
Tuesday, July 17, 2012, 16:00, John Wong, , targetboat (TaC coated), , Done, Sintering TaC coated regular- & D-endcaps
|
Tuesday, July 17, 2012, 15:45
Target boat is filled with TaC coated regular- and D-endcaps.
The boat is wrapped with a Ta heat-shield. |
|