ID |
Date |
Author |
Target Material |
Target Oven W.O# |
Source |
Status |
Subject |
Text |
 |
20
|
Tuesday, May 15, 2012, 17:06 |
John Wong | | | | Problems resolved | TBHT power supply faulty | Tuesday, May 15, 2012, 17:03
The tube heater power supply current
readback and setpoint are not matching. Ray |
|
19
|
Tuesday, May 15, 2012, 17:03 |
John Wong | | | | Problems | TBHT cooling line leaky | Tuesday, May 15, 2012, 17:00
It was found that there were water
droplets from the TBHT cooling line. The |
|
21
|
Wednesday, May 16, 2012, 14:04 |
John Wong | | | | Problems resolved | TBHT cooling line leaky |
|
|
584
|
Tuesday, June 21, 2022, 09:48 |
Darwin Ortiz Rosales | SiC | 37978-1 | HP-FEBIAD | Done | T-220617 sintering | Tuesday, June 21, 2022, 09:43
Total number of foils: |
|
578
|
Tuesday, June 07, 2022, 07:31 |
Darwin Ortiz Rosales | SiC | 42464-2 | HP-FEBIAD | Done | T-220524 Sintering SiC | Tuesday, June 07, 2022, 07:19
Total number of foils: |
|
576
|
Wednesday, May 18, 2022, 09:59 |
Darwin Ortiz Rosales | SiC | 44692-9 | HP-FEBIAD | Done | T-220516 Sintering SiC | Wednesday, May 18, 2022, 09:46
Total number of foils: |
|
605
|
Thursday, November 24, 2022, 11:08 |
John Wong | TiC | | TARGET BOAT | Done | Synthesis of TiC fibrous disc (TiO2/PAN only) | Thursday, November 24, 2022, 11:01
Target container contains one disc
of e-spun TiO2/PAN fibrous disc, (Ref sample |
 |
595
|
Tuesday, October 18, 2022, 13:59 |
Hannah Toy | TiC | Target boat (tube) | TARGET BOAT | Done | Synthesis of TiC | Tuesday, October 18, 2022, 13:52
38 pieces of samples made of TiO2/C/PVP
loaded into a target boat wrapped with 2 |
|
596
|
Wednesday, October 19, 2022, 09:50 |
John Wong | TiC | Target boat (tube) | TARGET BOAT | Done | Synthesis of TiC |
|
   |
635
|
Monday, June 05, 2023, 14:52 |
Aaron Schmidt | | | | | Swapped turbo pumps. | Previous TP would only spin up to
4KRPM. New TP installed.
Monday, June 05, 2023, 14:50: Roughing. |
|
128
|
Thursday, March 27, 2014, 18:04 |
John Wong | | | TARGET BOAT | In progress | Studying WC sintering on Ta surface | Thursday, March 27, 2014, 17:38
TEST #1
WC slurry was prepared in non-aqueous |
|
75
|
Tuesday, May 14, 2013, 17:15 |
John Wong | Empty | 38481-6 | HP-FEBIAD | Done | SinteringTaC coating | Tuesday, May 14, 2013, 17:04
Target oven is coated with TaC, and
wrapped with 3-Ta heat shields. |
|
190
|
Wednesday, May 06, 2015, 13:59 |
Laura Lambert | | 40282-4 | TARGET BOAT | Done | Sintering two different ZrC samples | Wednesday, May 06, 2015, 13:54
Two different samples of ZrC are
wrapped in graphite sheet and loaded into |
|
192
|
Wednesday, May 13, 2015, 16:01 |
Laura Lambert | | 40282-4 | TARGET BOAT | Done | Sintering three different ZrC samples | Wednesday, May 13, 2015, 15:21
Three different samples of ZrC |
|
130
|
Thursday, May 29, 2014, 18:16 |
Cameron Hodgins | | | TARGET BOAT | In progress | Sintering several carbides on tantalum foil backing | Purpose: Sinter one sample of each of TiC,
VC, Cr3C2, ZrC, NbC, Mo2C, TaC, and WC on
5x10 mm tantalum foil to see if the samples |
|
131
|
Friday, May 30, 2014, 13:15 |
Cameron Hodgins | | | | In progress | Sintering several carbides on tantalum foil backing | Pressure down to 7.1e-7 Torr. Water
valve to heat shield was opened; pressure
remained stable. |
|
132
|
Friday, June 06, 2014, 16:01 |
Cameron Hodgins | | | TARGET BOAT | In progress | Sintering several carbides on tantalum foil backing | Auto-ramp started. Max current = 500 A,
voltage = 11.05 V. Current is being increased
at 2 A/min. In the first 20 minutes, the |
|
133
|
Monday, June 09, 2014, 13:56 |
Cameron Hodgins | | | TARGET BOAT | In progress | Sintering several carbides on tantalum foil backing | Manually changed current from 500 to 615
A, monitoring the temperature. Temperature
went from 1657 C up to 1838 C. Pressure increased |
|
134
|
Monday, June 09, 2014, 17:15 |
Cameron Hodgins | | | TARGET BOAT | In progress | Sintering several carbides on tantalum foil backing | Target boat is now being cooled at
1 A/min from the starting point (616 A) down
to 0 A. |
|
317
|
Wednesday, August 24, 2016, 17:07 |
John Wong | SiC | 39814-V2-1 | LP-IG-LIS | Done | Sintering process for SiC#34 (2nd round) | Wednesday, August 24, 2016, 17:05
Target container was previously coated
with TaC and sintered up to 1900C at 420A/7.01V |
10x |