Thursday, August 20, 2015, 10:07, Laura Lambert, Ta, , HP-SIS, In progress, Conditioning Ta#46 Target
|
John Wong wrote:
|
Tuesday, August 25, 2015, 11:54, Laura Lambert, Empty, , HP-FEBIAD, In progress, Sintering TaC coating container for SiC Target
|
Tuesday, August 25, 2015, 11:50
Container coated with TaC using new method: Ends tapped off, with liquid poured in and swirled around entire container, then poured back
out - 'flushing technique' |
Tuesday, September 01, 2015, 17:20, John Wong, SiC, 39530-5, HP-FEBIAD, In progress, Sintering SiC#32
|
Tuesday, September 01, 2015, 17:16
Target container contains 533 discs of SiC with packed length of 17cm.
Mass of 533 discs SiC(green) = 57.8979g |
Wednesday, September 02, 2015, 11:28, Laura Lambert, SiC, 39530-5, HP-FEBIAD, In progress, Sintering SiC#32
|
John Wong wrote:
Tuesday, September 01, 2015, 17:16 |
Tuesday, September 08, 2015, 15:56, John Wong, SiC, 39530-5, HP-FEBIAD, In progress, Sintering SiC#32
|
Laura Lambert wrote:
|
Wednesday, September 09, 2015, 18:24, John Wong, SiC, 39530-5, HP-FEBIAD, In progress, Re-conditioning SiC#32
|
John Wong wrote:
|
Thursday, September 10, 2015, 09:58, Laura Lambert, SiC, 39530-5, HP-FEBIAD, In progress, Re-conditioning SiC#32
|
John Wong wrote:
|
Thursday, September 24, 2015, 09:48, Laura Lambert, Empty, 41077-5, , In progress, Sintering TaC coating container for UCx Target
|
Thursday, September 24, 2015, 08:39
IGP1 = 6.5e-7Torr
HS water valves opened, no leaks detected. |
Tuesday, October 06, 2015, 15:18, John Wong, Empty, 41077-5, LP-SIS, In progress, Test#1: Measuring temp with thermocouple (centre) & 2C-IR
|
John Wong wrote:
|
Thursday, October 08, 2015, 12:26, John Wong, Empty, 41077-5, LP-SIS, In progress, Test#2: Measuring temp with thermocouple (away from centre) & 2C-IR
|
John Wong wrote:
|
Wednesday, October 21, 2015, 17:39, John Wong, Empty, 41077-3, LP-SIS, In progress, Sintering TaC on LPSIS (small block) container
|
Wednesday, October 21, 2015, 17:35
This container is prepared for a backup UCx target (otherwise it will be used for development purposes).
The container is coated with TaC; one layer of Ta-heat shield is used. |
Thursday, October 22, 2015, 11:41, Laura Lambert, Empty, 41077-3, LP-SIS, In progress, Sintering TaC on LPSIS (small block) container
|
John Wong wrote:
Wednesday, October 21, 2015, 17:35 |
Thursday, October 22, 2015, 17:10, John Wong, Empty, 41077-3, LP-SIS, In progress, Sintering TaC on LPSIS (small block) container
|
Laura Lambert wrote:
|
Thursday, November 05, 2015, 16:20, Laura Lambert, , 41077-3, LP-SIS, In progress, Sintering TaC coating on 'temporary endcaps' springs
|
Thursday, November 05, 2015, 16:19
Springs coated with TaC and loaded into container for sintering.
3x Ta heat shield. |
Monday, November 09, 2015, 12:56, John Wong, , 41077-3, LP-SIS, In progress, Sintering TaC coating on 'temporary endcaps' springs (Slope changed to 1.04)
|
Laura Lambert wrote:
Thursday, November 05, 2015, 16:19 |
Tuesday, December 01, 2015, 11:35, Anders Mjos, Empty, 41077-5, LP-SIS, In progress, Test#2: Measuring temp with thermocouple (away from centre) & 2C-IR
|
Data from thermocouple attached. Raw data and Excel sheet with plot. |
Thursday, January 07, 2016, 09:19, Aurelia Laxdal, Ta, 41369-5, HP-SIS, In progress, Temperature measurements
|
Temperature measurements in progress this week for Ta HP-SIS.
See attachment for the current settings and rampings of the TGHT/TBHT for the temperature measurements taken on Jan. 9-10, 2016 .
Note: TBHT PS tripped off on Jan. 9, 2016 (see first page of the attached file) and couldn't turn it ON again over the week-end. |
Tuesday, February 16, 2016, 14:02, Laura Lambert, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube]
|
Tuesday, February 16, 2016, 14:19
coated with TaC yesterday and let dry overnight.
wrapped with one long Ta heat shield - wrapped around tube 3x, with Ta wire to offset Ta foil away from container |
Thursday, February 18, 2016, 13:22, John Wong, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube]
|
Laura Lambert wrote:
Tuesday, February 16, 2016, 14:19 |
Sunday, March 13, 2016, 14:58, Aurelia Laxdal, Ta, 41790-1, LP-SIS, In progress, Ta#47 LP-SIS (with new center block) conditioning
|
Started Ta#47 heating at Evap2 using the autoramp program. The TGHT current is setup to go to 300A (for now) and the TBHT to 230A (final value). |
|