19
|
Tuesday, May 15, 2012, 17:03 |
John Wong | | | | Problems | TBHT cooling line leaky | Tuesday, May 15, 2012, 17:00
It was found that there were water
droplets from the TBHT cooling line. The |
|
|
20
|
Tuesday, May 15, 2012, 17:06 |
John Wong | | | | Problems resolved | TBHT power supply faulty | Tuesday, May 15, 2012, 17:03
The tube heater power supply current
readback and setpoint are not matching. Ray |
|
|
21
|
Wednesday, May 16, 2012, 14:04 |
John Wong | | | | Problems resolved | TBHT cooling line leaky |
|
|
|
26
|
Tuesday, May 22, 2012, 16:45 |
Nikita Bernier | BeO | Target boat #2 | | Done | Sintering BeO pellets #3 |
|
|
|
27
|
Wednesday, May 23, 2012, 17:45 |
John Wong | BeO | Target boat #2 | | Done | Sintering BeO pellets #3 |
|
|
|
28
|
Monday, May 28, 2012, 11:15 |
John Wong | | | | Problems | Chiller is leaking water | Monday, May 28, 2012, 11:08
It was discovered this morning that
the Evaporator #2 chiller was leaking water |
|
|
29
|
Tuesday, May 29, 2012, 15:43 |
Nikita Bernier | BeO | Target boat #2 | | Failed | Sintering BeO pellets #3 |
|
|
|
31
|
Wednesday, June 20, 2012, 17:29 |
Nikita Bernier | NiO | Ta target boat | | Done | NiO development | Wednesday, June 20, 2012, 17:23
New Target boat, with no coating,
wrapped with a 0.002 inches thick Ta foil, |
|
|
32
|
Wednesday, June 20, 2012, 22:33 |
John Wong | NiO | Ta target boat | | Done | NiO development |
|
|
|
33
|
Thursday, June 21, 2012, 18:13 |
John Wong | NiO | Ta target boat | | Failed | NiO development - Container broke! |
|
|
|
34
|
Thursday, July 12, 2012, 17:55 |
John Wong | NiO | targetboat (TaC coated) | | Maintenance | NiO development- test#2 | Thursday, July 12, 2012, 17:29
NiO was sprayed on Ni foil.
Average/discs: mass= 0.075g, thickness=0.076mm, |
|
|
35
|
Tuesday, July 17, 2012, 16:00 |
John Wong | | targetboat (TaC coated) | | Done | Sintering TaC coated regular- & D-endcaps | Tuesday, July 17, 2012, 15:45
Target boat is filled with TaC coated
regular- and D-endcaps. |
|
|
38
|
Monday, July 30, 2012, 15:42 |
John Wong | | | | Problems | Chiller maybe leaky | Monday, July 30, 2012, 15:38
The evaporator was used for the processing
the NiO target for 8 days and it was discovered |
|
|
39
|
Friday, August 10, 2012, 19:57 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating | Friday, August 10, 2012, 19:54
|
|
|
40
|
Saturday, August 11, 2012, 19:21 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
|
|
41
|
Monday, August 13, 2012, 13:50 |
Nikita Bernier | | | | Done | Sintering Ta foil with TaO coating |
|
|
|
42
|
Tuesday, August 14, 2012, 15:11 |
John Wong | | | | Maintenance | Replacing Cu-heatshield insulators | Tuesday, August 14, 2012, 15:01
The Cu-heatshield insulators are
broken due to prolong heating time during |
|
|
44
|
Tuesday, August 14, 2012, 17:11 |
John Wong | | | | Failed | Sintering Ta2O5 coating on Ta foil failed |
|
|
|
46
|
Monday, September 24, 2012, 15:12 |
Nikita Bernier | TaC | | | Done | Sintering Ta foil with TaC coating | Monday, September 24, 2012, 15:01
The target boat with TaC coating
is being used again. The inside of the boat |
|
|
47
|
Monday, September 24, 2012, 18:09 |
Nikita Bernier | TaC | | | Done | Sintering Ta foil with TaC coating |
|
|
|