Entry  Monday, November 23, 2015, 14:36, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, temp measurements with no h.s on HP-FEBIAD container temp_measurements.xlsx
Monday, November 23, 2015, 14:29
No heat shields.
Container empty.
Entry  Monday, November 30, 2015, 15:38, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, emissivity measurements with no h.s on HP-FEBIAD container emissivity_measurements.xlsx
 Monday, November 30, 2015, 15:37
No heat shields.
Container empty.
    Reply  Tuesday, December 01, 2015, 11:35, Anders Mjos, Empty, 41077-5, LP-SIS, In progress, Test#2: Measuring temp with thermocouple (away from centre) & 2C-IR 2015-10-08_Small_Centre_Block.xlsx2015-10-08.4ch2015-10-06.4ch2015-10-06_Small_Centre_Block.xlsx
 Data from thermocouple attached. Raw data and Excel sheet with plot.
Entry  Monday, December 07, 2015, 09:06, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, emissivity measurements with no h.s on HP-FEBIAD container - round2 
 Monday, December 07, 2015, 09:04
No heat shields.
Container empty.
Entry  Friday, February 12, 2016, 11:09, Laura Lambert, Empty, 41077-1, LP-SIS, Done, sintering TaC coated small center block container 
 Friday, February 12, 2016, 11:01
Container coated with TaC with new method - ends tapped off,  liquid poured/swirled
around container, then poured back out - 'flushing technique'.
Entry  Tuesday, February 16, 2016, 14:02, Laura Lambert, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube] 
 Tuesday, February 16, 2016, 14:19
coated with TaC yesterday and let dry overnight.
wrapped with one long Ta heat shield - wrapped around tube 3x, with Ta wire to offset Ta foil away from container
    Reply  Thursday, February 18, 2016, 13:22, John Wong, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube] 


    
        
            Laura Lambert wrote:
        
        
            
             Tuesday, February 16, 2016, 14:19
    Reply  Thursday, February 18, 2016, 17:21, Laura Lambert, Empty, 40202-5, TARGET BOAT, Done, sintered TaC coating on target boat [container style with no ionizer tube] 


    
        
            John Wong wrote:
        
        
            
            
            
Entry  Tuesday, April 26, 2016, 13:50, Laura Lambert, Empty, 40860-2, LP-IG-LIS, Done, sintering TaC coating on UCx#16 container TaC_coating_sintered1.jpgTaC_coating_sintered2.jpgTaC_coating_sintered3.jpg
Tuesday, April 26, 2016, 13:32
Container coated with TaC using 'flushing technique'.
Wrapped with 3 x Ta heat shields, incl center block - new method of each layer being one long
Entry  Wednesday, May 25, 2016, 11:40, Laura Lambert, Empty, 41369-4, HP-SIS, In progress, sintering TaC coating on SiC#33 container 
 Wednesday, May 25, 2016, 11:37
Container coated with TaC using 'flushing technique' [cleaned ionizer tube with acetone, so no
coating inside ionizer tube]
    Reply  Tuesday, May 31, 2016, 11:10, John Wong, Empty, 41369-4, HP-SIS, Done, sintering TaC coating on SiC#33 container 


    
        
            Laura Lambert wrote:
        
        
            
             Wednesday, May 25, 2016, 11:37
Entry  Monday, June 27, 2016, 11:08, Laura Lambert, Empty, 41790-3, LP-SIS, Done, sintering TaC coating on UCx#17 container LP-SIS_post_sintering_TaC(3).jpgLP-SIS_post_sintering_TaC(4).jpg
 Monday, June 27, 2016, 11:07
Container coated with TaC using 'flushing technique'.
Wrapped with 3 x Ta heat shields, incl center block - new method of each layer being one long
Entry  Friday, July 15, 2016, 11:52, Laura Lambert, Empty, 40860-3, LP-IG-LIS, Done, sintering TaC coating on SiC#34 container Evernote_Camera_Roll_20160524_134232.jpgEvernote_Camera_Roll_20160524_134233.jpgEvernote_Camera_Roll_20160524_1342331.jpgEvernote_Camera_Roll_20160524_1342332.jpgsnapshot_of_striptool_sintering_TaC_coating.JPG
 Friday, July 15, 2016, 11:49
Container previously coated with TaC using 'flushing technique', cleaned ionizer tube with acetone,
so no coating inside ionizer tube
Entry  Wednesday, August 17, 2016, 17:31, Laura Lambert, Empty, 39814-V2-1, LP-IG-LIS, In progress, sintering TaC coating on SiC#34 container...round2 leak.JPGwater_leak.JPEG
 Wednesday, August 17, 2016, 17:30
Container coated with TaC using 'flushing technique', cleaned ionizer tube with acetone, so no
coating inside ionizer tube
    Reply  Tuesday, August 23, 2016, 12:15, John Wong, Empty, 39814-V2-1, LP-IG-LIS, Done, sintering TaC coating on SiC#34 container...round2 


    
        
            Laura Lambert wrote:
        
        
            
             Wednesday, August 17, 2016, 17:30
Entry  Wednesday, September 07, 2016, 15:02, John Wong, Empty, 39530-9, HP-SIS, In progress, Sintering TaC coating container for SiC Target  coating_chipped_off.JPGautoTaC_sintering_20.JPEGcoating_chipped_off_2.JPG
 Wednesday, September 07, 2016, 14:45
Container was previously coated with TaC solution and wrapped with 1-full length layer of Ta- heat shield around the fins.  
Chamber is being pumped down.  Vac at 5.6e-7 Torr before HS water valves were open; no leaks were detected. 
    Reply  Monday, September 12, 2016, 17:22, John Wong, Empty, 39530-9, HP-SIS, Failed, TaC coating chipped off Screen_Shot_2016-09-12_at_4.52.53_PM.png


    
        
            John Wong wrote:
        
        
            
             Wednesday, September 07, 2016, 14:45
    Reply  Monday, September 12, 2016, 17:27, John Wong, Empty, 39530-9, HP-SIS, Done, RUSH. Round 2: Sinering TaC coating  Screen_Shot_2016-09-14_at_5.05.08_PM.pngScreen_Shot_2016-09-14_at_5.03.48_PM.png


    
        
            John Wong wrote:
        
        
            
            
            
Entry  Wednesday, September 28, 2016, 17:09, Laura Lambert, Empty, 41790-6, LP-SIS, Done, sintering TaC coating on UCx container sintering_TaC_coating.xlsxsintering_TaC_coating.JPGsintering_TaC_coating2.JPGsintering_TaC_coating-combo_of_both_pics.JPG
 Wednesday, September 28, 2016, 17:08
Container coated with TaC using 'flushing technique' today, cleaned ionizer tube with acetone,
no coating inside ionizer tube
Entry  Thursday, December 01, 2016, 16:08, Laura Lambert, Empty, 42218-12, LP-SIS, Done, sintering TaC coating on UCx#19 container 
 Thursday, December 01, 2016, 16:06
Container coated with TaC using 'flushing technique' and let dry overnight.