Thursday, February 09, 2017, 11:49, Laura Lambert, , , , Maintenance, New heatshield with flexible water lines
|
Thursday, February 09, 2017, 11:47
A new heatshield with flexible water lines has been put into evap2 last Friday Feb3rd
|
Monday, February 06, 2017, 11:17, Anders Mjos, , , , Problems resolved, IOC restart after power outagae
|
Dave Morris did a remote restart of the IOC after the outage. Turbo pump started. |
Tuesday, January 31, 2017, 16:03, Laura Lambert, Empty, 39530-10, HP-FEBIAD, Done, Sintering TaC coated container for backup
|
Tuesday, January 31, 2017, 13:43
Container coated with TaC using new method: Ends taped off, with liquid poured in and swirled
around entire container, then poured back out - 'flushing technique' |
Tuesday, December 20, 2016, 15:04, Laura Lambert, , , , Maintenance, RETURN and SUPPLY valves CLOSED for xmas break
|
Tuesday, December 20, 2016, 15:05
confirmed ~full tank of Ar for glove box --> ~1600psi |
Friday, December 16, 2016, 14:14, Laura Lambert, Ta, 39530-3, LP-FEBIAD, Done, Conditioning Ta FEBIAD target for shutdown tests
|
Friday, December 16, 2016, 14:08
Target consists of 470 discs.
Total packed length 3.4cm [exactly 7.8cm space on both sides] |
Thursday, December 01, 2016, 16:08, Laura Lambert, Empty, 42218-12, LP-SIS, Done, sintering TaC coating on UCx#19 container
|
Thursday, December 01, 2016, 16:06
Container coated with TaC using 'flushing technique' and let dry overnight.
Cleaned ionizer tube with acetone, no coating inside ionizer tube |
Tuesday, November 22, 2016, 15:58, Laura Lambert, Nb, 40282-3, TARGET BOAT, Done, Conditioning Nb samples for Doug
|
Tuesday, November 22, 2016, 15:53
Target boat has a layer of niobium foil on the bottom of the boat.
A niobium foil has been made with slots to hold samples [similar to when sintering endcaps] *See |
Tuesday, November 15, 2016, 16:51, John Wong, np-SiC, , TARGET BOAT, In progress, Heat-treatment: Beta-SiC (1um) fiber mats - SAMPLE ID: A1
|
Tuesday, November 15, 2016, 16:48
Three samples were prepared (see my logbook#1 page 3, preparing for carbonization).
One layer of Ta foil was used to wrap around the target boat. |
Thursday, November 17, 2016, 11:15, Laura Lambert, np-SiC, , TARGET BOAT, In progress, Heat-treatment: Beta-SiC (1um) fiber mats - SAMPLE ID: A1
|
John Wong wrote:
Tuesday, November 15, 2016, 16:48 |
Friday, November 18, 2016, 17:28, John Wong, np-SiC, , TARGET BOAT, Done, Heat-treatment: Beta-SiC (1um) fiber mats - SAMPLE ID: A1
|
Laura Lambert wrote:
|
Monday, October 24, 2016, 17:52, John Wong, np-SiC, , TARGET BOAT, Done, Thermo test of np-SiC raw powder
|
Monday, October 24, 2016, 17:43
Two samples were prepared and loaded into the target boat with 1 layer of heat-shied as shown in the attachment#1.
Ingredients used: np-SiC and very small about of 5% PVA to hold the powder together. |
Thursday, October 13, 2016, 18:05, Laura Lambert, Ta, 41790-5, LP-SIS, In progress, Temperature measurements for Ta#50
|
Thursday, October 13, 2016, 18:04
Target loaded into evap2
No heat shields. |
Saturday, October 15, 2016, 12:42, Aurelia Laxdal, Ta, 41790-5, LP-SIS, In progress, Temperature measurements for Ta#50
|
Laura Lambert wrote:
Thursday, October 13, 2016, 18:04 |
Sunday, October 16, 2016, 17:55, Aurelia Laxdal, Ta, 41790-5, LP-SIS, In progress, Temperature measurements for Ta#50
|
Aurelia Laxdal wrote:
|
Tuesday, October 18, 2016, 09:23, Laura Lambert, Ta, 41790-5, LP-SIS, Done, Temperature measurements for Ta#50
|
Aurelia Laxdal wrote:
|
Friday, October 07, 2016, 16:42, Laura Lambert, Ta, 41790-5, LP-SIS, In progress, Conditioning Ta#50
|
Friday, October 07, 2016, 16:40
Target consists of 470 discs.
Total packed length 3.4cm [exactly 7.8cm space on both sides] |
Wednesday, October 12, 2016, 21:18, John Wong, Ta, 41790-5, LP-SIS, In progress, Conditioning Ta#50
|
Laura Lambert wrote:
Friday, October 07, 2016, 16:40 |
Thursday, October 13, 2016, 17:32, Laura Lambert, Ta, 41790-5, LP-SIS, Done, Conditioning Ta#50
|
John Wong wrote:
|
Wednesday, September 28, 2016, 17:09, Laura Lambert, Empty, 41790-6, LP-SIS, Done, sintering TaC coating on UCx container
|
Wednesday, September 28, 2016, 17:08
Container coated with TaC using 'flushing technique' today, cleaned ionizer tube with acetone,
no coating inside ionizer tube |
Thursday, September 15, 2016, 16:37, Laura Lambert, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35
|
Thursday, September 15, 2016, 16:23
Target container contains 487 discs of SiC
Target packed length = 16cm. |
Monday, September 19, 2016, 18:48, John Wong, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35 - Change OMEGA/MiKRON slopes
|
Laura Lambert wrote:
Thursday, September 15, 2016, 16:23 |
Tuesday, September 20, 2016, 15:40, Laura Lambert, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35
|
John Wong wrote:
|
Thursday, September 22, 2016, 12:14, John Wong, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35
|
Laura Lambert wrote:
|
Monday, September 26, 2016, 13:49, Laura Lambert, SiC, 39530-9, HP-FEBIAD, Done, Sintering SiC#35
|
John Wong wrote:
|
Wednesday, September 07, 2016, 15:02, John Wong, Empty, 39530-9, HP-SIS, In progress, Sintering TaC coating container for SiC Target
|
Wednesday, September 07, 2016, 14:45
Container was previously coated with TaC solution and wrapped with 1-full length layer of Ta- heat shield around the fins.
Chamber is being pumped down. Vac at 5.6e-7 Torr before HS water valves were open; no leaks were detected. |
Monday, September 12, 2016, 17:22, John Wong, Empty, 39530-9, HP-SIS, Failed, TaC coating chipped off
|
John Wong wrote:
Wednesday, September 07, 2016, 14:45 |
Monday, September 12, 2016, 17:27, John Wong, Empty, 39530-9, HP-SIS, Done, RUSH. Round 2: Sinering TaC coating
|
John Wong wrote:
|
Monday, August 08, 2016, 15:22, Laura Lambert, SiC, 40860-3, LP-IG-LIS, Problems, Conditioning SiC#34
|
Monday, August 08, 2016, 15:19
Previously sintered over weekend [see elog i.d 311]
Target container contains 471 discs of SiC [6 x 5 packs + 441 single discs] |
Tuesday, August 30, 2016, 15:25, John Wong, SiC, 40860-3, LP-IG-LIS, Problems, Conditioning SiC#34. Note about the p/s voltage
|
Laura Lambert wrote:
Monday, August 08, 2016, 15:19 |
Wednesday, August 24, 2016, 17:07, John Wong, SiC, 39814-V2-1, LP-IG-LIS, Done, Sintering process for SiC#34 (2nd round) 10x
|
Wednesday, August 24, 2016, 17:05
Target container was previously coated with TaC and sintered up to 1900C at 420A/7.01V
Container is loaded with beta-SiC 432 discs at 16cm in length. |
Wednesday, August 17, 2016, 17:31, Laura Lambert, Empty, 39814-V2-1, LP-IG-LIS, In progress, sintering TaC coating on SiC#34 container...round2
|
Wednesday, August 17, 2016, 17:30
Container coated with TaC using 'flushing technique', cleaned ionizer tube with acetone, so no
coating inside ionizer tube |
Tuesday, August 23, 2016, 12:15, John Wong, Empty, 39814-V2-1, LP-IG-LIS, Done, sintering TaC coating on SiC#34 container...round2
|
Laura Lambert wrote:
Wednesday, August 17, 2016, 17:30 |
Thursday, August 18, 2016, 10:37, Anders Mjos, , , , Maintenance, New cooling lines for Heat Shield
|
Dan made a set of new cooling lines for the Source Tray Heat Shield cooling yesterday. No joints on the lines. Use same VCR fitting 3/8 -> 1/4"
as for the Heat Shield. The old lines had worn threads on the male VCR nut. |
Friday, August 12, 2016, 11:08, Laura Lambert, , , , Maintenance, NEW PUMP FOR GLOVE BOX
|
Wednesday, August 03, 2016, 16:16
Tues July 26th had some problems with the transfer chamber
Transfer chamber was not going below -20in pressure, when usually it will drop all the way to -30in |
Tuesday, August 02, 2016, 13:56, Laura Lambert, SiC, 40860-3, LP-IG-LIS, Done, Sintering SiC#34
|
Tuesday, August 02, 2016, 13:41
Target container contains 471 discs of SiC [6 x 5 packs + 441 single discs]
Target packed length = 16cm. |
|