ID |
Date |
Author |
Target Material |
Target Oven W.O# |
Source |
Status |
Subject |
Text |
|
|
66
|
Thursday, April 11, 2013, 14:20 |
John Wong | Empty | 39165-6 | LP-SIS | Done | Coating target oven /w TaC & sintering for UCx#6 | Monday, April 08, 2013, 17:39
Target container is coated with TaC;
the container will be used for the UCx#6 |
|
|
79
|
Monday, July 22, 2013, 15:03 |
John Wong | Empty | 38634-7 | LP-SIS | Done | Sintering empty target oven coated with TaC for UCx#7 | Monday, July 22, 2013, 15:00
Target container is coated with TaC
- this container will be used for UCx#7. |
|
|
91
|
Friday, October 04, 2013, 16:21 |
John Wong | Empty | | LP-SIS | Done | Sintering TaC coating on a LP target container to be used for C-grv tube test | Friday, October 04, 2013, 15:37
A LP target container is coated with
TaC. The container is wrapped with |
|
|
97
|
Wednesday, January 15, 2014, 17:45 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container | Wednesday, January 15, 2014, 17:30
Target container is coated with TaC.
No Ta-heat shields are used. |
|
|
98
|
Thursday, January 16, 2014, 13:06 |
Laura Lambert | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
|
99
|
Friday, January 17, 2014, 09:34 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
|
100
|
Friday, January 17, 2014, 10:18 |
Laura Lambert | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
|
101
|
Friday, January 17, 2014, 12:52 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
|
102
|
Monday, January 20, 2014, 16:30 |
Laura Lambert | Empty | 39165-9 | LP-SIS | Done | Sintering TaC coating container |
|
|
|
116
|
Friday, January 31, 2014, 12:10 |
Laura Lambert | Empty | 39165-10 | LP-SIS | Done | Sintering TaC coating container for Ta? | Friday, January 31, 2014, 11:28
Target container is coated with TaC.
The container is wrapped with 3 x |
|
|
135
|
Friday, June 13, 2014, 14:57 |
Laura Lambert | Ta | 40282-2 | LP-SIS | In progress | Conditioning Ta#43 target | Friday, June 13, 2014, 14:53
Container is filled with 400 discs
of Ta foils; target length = 5.2cm; |
|
|
136
|
Monday, June 16, 2014, 17:42 |
John Wong | Ta | 40282-2 | LP-SIS | In progress | Conditioning Ta#43 target |
|
|
|
137
|
Tuesday, June 17, 2014, 10:14 |
Laura Lambert | Ta | 40282-2 | LP-SIS | Done | Conditioning Ta#43 target |
|
|
|
143
|
Wednesday, July 23, 2014, 15:07 |
John Wong | Empty | 40282-3 | LP-SIS | In progress | Sintering TaC coated target container | Wednesday, July 23, 2014, 15:07
Target container is coated with TaC.
No Ta-heat shields are used. |
|
|
144
|
Monday, July 28, 2014, 10:52 |
Laura Lambert | Empty | 40282-3 | LP-SIS | Done | Sintering TaC coated target container |
|
|
|
145
|
Monday, July 28, 2014, 15:06 |
Laura Lambert | | 40282-3 | LP-SIS | In progress | Sintering ZrC# 6 target | Monday, July 28, 2014, 14:41
Total number of foils: 445 discs
Total mass of materials [incl graphite |
|
|
146
|
Tuesday, July 29, 2014, 11:23 |
John Wong | | 40282-3 | LP-SIS | In progress | Sintering ZrC# 6 target |
|
|
|
147
|
Friday, August 01, 2014, 11:47 |
Peter Kunz | | 40282-3 | LP-SIS | In progress | ZrC #6 conditioning | The maximum current of 580A was reached
at 9:15.
TGHT:RDCUR 578 A |
|
|
148
|
Friday, August 01, 2014, 13:27 |
Peter Kunz | | 40282-3 | LP-SIS | In progress | ZrC #6 conditioning | Target was conditioned for 4 hours at 580A.
Initiating ramp-down sequence @ 2A/min
|
|
|
149
|
Tuesday, August 05, 2014, 12:01 |
Laura Lambert | | 40282-3 | LP-SIS | Done | ZrC #6 conditioning |
|
|