Friday, June 13, 2014, 14:57, Laura Lambert, Ta, 40282-2, LP-SIS, In progress, Conditioning Ta#43 target
|
Friday, June 13, 2014, 14:53
Container is filled with 400 discs of Ta foils; target length = 5.2cm;
Total mass ( Ta foils + wire) = 45.92g |
Monday, June 16, 2014, 17:42, John Wong, Ta, 40282-2, LP-SIS, In progress, Conditioning Ta#43 target
|
Laura Lambert wrote:
Friday, June 13, 2014, 14:53 |
Tuesday, June 17, 2014, 10:14, Laura Lambert, Ta, 40282-2, LP-SIS, Done, Conditioning Ta#43 target
|
John Wong wrote:
|
Thursday, April 06, 2017, 13:16, Laura Lambert, Empty, 40282-2, TARGET BOAT, Done, Sintering TaC coating on evap1 target boat
|
Laura Lambert wrote:
|
Tuesday, February 16, 2016, 14:02, Laura Lambert, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube]
|
Tuesday, February 16, 2016, 14:19
coated with TaC yesterday and let dry overnight.
wrapped with one long Ta heat shield - wrapped around tube 3x, with Ta wire to offset Ta foil away from container |
Thursday, February 18, 2016, 13:22, John Wong, Empty, 40202-5, TARGET BOAT, In progress, sintered TaC coating on target boat [container style with no ionizer tube]
|
Laura Lambert wrote:
Tuesday, February 16, 2016, 14:19 |
Thursday, February 18, 2016, 17:21, Laura Lambert, Empty, 40202-5, TARGET BOAT, Done, sintered TaC coating on target boat [container style with no ionizer tube]
|
John Wong wrote:
|
Thursday, September 26, 2013, 15:17, John Wong, Empty, 39814-VI-?, LP-IG-LIS, Done, Sintering empty target oven coated with TaC for UCx#8
|
Thursday, September 26, 2013, 13:04
The LP-IG-LIS target container is coated with TaC.
Container is wrapped with 3 layers of Ta heat shield and about to go through the sintering process. |
Wednesday, August 17, 2016, 17:31, Laura Lambert, Empty, 39814-V2-1, LP-IG-LIS, In progress, sintering TaC coating on SiC#34 container...round2 
|
Wednesday, August 17, 2016, 17:30
Container coated with TaC using 'flushing technique', cleaned ionizer tube with acetone, so no
coating inside ionizer tube |
Tuesday, August 23, 2016, 12:15, John Wong, Empty, 39814-V2-1, LP-IG-LIS, Done, sintering TaC coating on SiC#34 container...round2
|
Laura Lambert wrote:
Wednesday, August 17, 2016, 17:30 |
Wednesday, August 24, 2016, 17:07, John Wong, SiC, 39814-V2-1, LP-IG-LIS, Done, Sintering process for SiC#34 (2nd round) 10x
|
Wednesday, August 24, 2016, 17:05
Target container was previously coated with TaC and sintered up to 1900C at 420A/7.01V
Container is loaded with beta-SiC 432 discs at 16cm in length. |
Monday, November 23, 2015, 14:36, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, temp measurements with no h.s on HP-FEBIAD container
|
Monday, November 23, 2015, 14:29
No heat shields.
Container empty. |
Monday, November 30, 2015, 15:38, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, emissivity measurements with no h.s on HP-FEBIAD container
|
Monday, November 30, 2015, 15:37
No heat shields.
Container empty. |
Monday, December 07, 2015, 09:06, Laura Lambert, Empty, 39530-9, HP-FEBIAD, Done, emissivity measurements with no h.s on HP-FEBIAD container - round2
|
Monday, December 07, 2015, 09:04
No heat shields.
Container empty. |
Wednesday, September 07, 2016, 15:02, John Wong, Empty, 39530-9, HP-SIS, In progress, Sintering TaC coating container for SiC Target  
|
Wednesday, September 07, 2016, 14:45
Container was previously coated with TaC solution and wrapped with 1-full length layer of Ta- heat shield around the fins.
Chamber is being pumped down. Vac at 5.6e-7 Torr before HS water valves were open; no leaks were detected. |
Monday, September 12, 2016, 17:22, John Wong, Empty, 39530-9, HP-SIS, Failed, TaC coating chipped off
|
John Wong wrote:
Wednesday, September 07, 2016, 14:45 |
Monday, September 12, 2016, 17:27, John Wong, Empty, 39530-9, HP-SIS, Done, RUSH. Round 2: Sinering TaC coating 
|
John Wong wrote:
|
Thursday, September 15, 2016, 16:37, Laura Lambert, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35
|
Thursday, September 15, 2016, 16:23
Target container contains 487 discs of SiC
Target packed length = 16cm. |
Monday, September 19, 2016, 18:48, John Wong, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35 - Change OMEGA/MiKRON slopes
|
Laura Lambert wrote:
Thursday, September 15, 2016, 16:23 |
Tuesday, September 20, 2016, 15:40, Laura Lambert, SiC, 39530-9, HP-FEBIAD, In progress, Sintering SiC#35
|
John Wong wrote:
|
|