Wednesday, May 13, 2015, 16:01, Laura Lambert, , 40282-4, TARGET BOAT, Done, Sintering three different ZrC samples
|
Wednesday, May 13, 2015, 15:21
Three different samples of ZrC are loaded into a target boat.
Sample A: ZrC + NO graphite |
Tuesday, May 19, 2015, 13:54, Laura Lambert, Empty, 41177-1, LP-SIS, Done, Sintering TaC coating container for ZrC
|
Tuesday, May 19, 2015, 13:33
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Tuesday, May 26, 2015, 13:05, Laura Lambert, Empty, 40282-5, TARGET BOAT, Done, Sintering TaC coating on Ta target boat
|
John Wong wrote:
|
Thursday, May 28, 2015, 17:50, John Wong, Endcaps, 40282-5, TARGET BOAT, Done, Sintering TaC coating on Ta endcaps - round 2
|
Laura Lambert wrote:
Thursday, May 28, 2015, 11:34 |
Friday, May 29, 2015, 11:18, Laura Lambert, Endcaps, 40282-5, TARGET BOAT, Done, Sintering TaC coating on Ta endcaps - round 2
|
John Wong wrote:
|
Tuesday, June 02, 2015, 13:05, John Wong, ZrC, 41177-1, LP-SIS, Done, Conditioning ZrC#7
|
John Wong wrote:
|
Wednesday, June 03, 2015, 10:47, Laura Lambert, ZrC, 41177-1, LP-SIS, Done, Conditioning ZrC#7
|
John Wong wrote:
|
Sunday, June 14, 2015, 09:40, John Wong, Empty, 40860-1, LP-IG-LIS, Done, Re-Sintering TaC coating container for UCx
|
John Wong wrote:
|
Monday, June 15, 2015, 15:30, John Wong, Empty, 41177-2, LP-SIS, Done, Re-Sintering TaC coating container for ZrC back-up
|
Laura Lambert wrote:
|
Tuesday, June 23, 2015, 10:18, Laura Lambert, Empty, 38817-6, HP-SIS, Done, RUSH! Sintering TaC coated container for SiC
|
John Wong wrote:
Monday, June 22, 2015, 13:00 |
Thursday, June 25, 2015, 16:13, Laura Lambert, SiC, 38817-6, HP-SIS, Done, RUSH! SiC backup target undergoes sintering process
|
John Wong wrote:
Tuesday, June 23, 2015, 12:21 |
Monday, June 29, 2015, 07:05, John Wong, ZrC, 41177-2, LP-SIS, Done, Sintering back-up ZrC
|
Laura Lambert wrote:
Thursday, June 25, 2015, 16:14 |
Monday, July 06, 2015, 16:30, Laura Lambert, Empty, 41369-2, LP-SIS, Done, Sintering TaC coating container
|
John Wong wrote:
|
Tuesday, August 04, 2015, 12:04, Laura Lambert, Ta, , TARGET BOAT, Done, Test for homogeneity: Sintering TaC coating on a Ta tube
|
John Wong wrote:
Friday, July 31, 2015, 15:39 |
Thursday, August 06, 2015, 15:45, Laura Lambert, Endcaps, , TARGET BOAT, Done, Sintering TaC coating on Ta endcaps
|
Thursday, August 06, 2015, 15:36
The endcaps are stacked together with a punched out disc of graphite foil placed in between each endcap for separation so endcaps won't fuse together.
The end caps are further wrapped in a larger piece of graphite foil to hold together as a tube [same method used in elogID # 158] |
Thursday, August 20, 2015, 17:15, John Wong, Ta, , HP-SIS, Done, Conditioning Ta#46 Target
|
Laura Lambert wrote:
|
Thursday, August 27, 2015, 16:37, John Wong, Empty, , HP-FEBIAD, Done, Sintering TaC coating container for SiC Target
|
Laura Lambert wrote:
Tuesday, August 25, 2015, 11:50 |
Thursday, September 10, 2015, 12:05, John Wong, SiC, 39530-5, HP-FEBIAD, Done, Re-conditioning SiC#32
|
Laura Lambert wrote:
|
Thursday, September 24, 2015, 12:18, John Wong, Empty, 41077-5, LP-SIS, Done, Sintering TaC coating container for UCx Target
|
Laura Lambert wrote:
Thursday, September 24, 2015, 08:39 |
Monday, October 26, 2015, 16:14, Laura Lambert, Empty, 41077-3, LP-SIS, Done, Sintering TaC on LPSIS (small block) container & temp measurements with 1xTa h.s
|
John Wong wrote:
|
|