95
|
Wednesday, November 06, 2013, 17:36 |
John Wong | TaC | Target Boat #2 | | In progress | Testing TaC matrix coating | The purpose of this experiment is to improve
the TaC coating mixed with other metals as
additives. The coating solution will |
|
97
|
Wednesday, January 15, 2014, 17:45 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container | Wednesday, January 15, 2014, 17:30
Target container is coated with TaC.
No Ta-heat shields are used. |
|
99
|
Friday, January 17, 2014, 09:34 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
101
|
Friday, January 17, 2014, 12:52 |
John Wong | Empty | 39165-9 | LP-SIS | In progress | Sintering TaC coating container |
|
|
108
|
Wednesday, January 22, 2014, 15:13 |
John Wong | Empty | 40282-4 | TARGET BOAT | | Sintering Ta target boat with TaC coating |
|
|
109
|
Wednesday, January 22, 2014, 18:22 |
John Wong | Empty | 40282-4 | TARGET BOAT | Problems | Sintering Ta target boat with TaC coating (IEVAP2:TBHT2 water signal problem) |
|
|
122
|
Friday, March 07, 2014, 22:25 |
John Wong | | 40282-3 | TARGET BOAT | Problems | Sintering TaC coated end caps |
|
|
123
|
Monday, March 10, 2014, 11:45 |
John Wong | | | | Maintenance | Replaced Backing Pump hose | Monday, March 10, 2014, 11:44
Rick replaced the backing pump hose
from 1.5" to 2.0" for better flow. |
|
124
|
Monday, March 10, 2014, 11:52 |
John Wong | | | | Problems resolved | The Chiller is down | Monday, March 10, 2014, 11:45
The chiller tripped off on March
7, 2014. |
|
125
|
Friday, March 21, 2014, 16:18 |
John Wong | TiC | 38817-8 | HP-SIS | In progress | Sintering TiC | Friday, March 21, 2014, 16:09
Target container is loaded with 360
Discs of TiC. |
|
127
|
Wednesday, March 26, 2014, 18:23 |
John Wong | TiC | 38817-8 | HP-SIS | Done | Sintering TiC#4 |
|
|
128
|
Thursday, March 27, 2014, 18:04 |
John Wong | | | TARGET BOAT | In progress | Studying WC sintering on Ta surface | Thursday, March 27, 2014, 17:38
TEST #1
WC slurry was prepared in non-aqueous |
|
129
|
Thursday, April 24, 2014, 18:13 |
John Wong | | | TARGET BOAT | Done | Tests: Sintering carbon Mesh coated with WC | Thursday, April 24, 2014, 17:25
The purpose of this experiment is
to see if the carbon mesh is suitable for |
|
136
|
Monday, June 16, 2014, 17:42 |
John Wong | Ta | 40282-2 | LP-SIS | In progress | Conditioning Ta#43 target |
|
|
140
|
Friday, June 20, 2014, 16:22 |
John Wong | SiC | 39530-8 | HP-FEBIAD | In progress | Conditioning SiC#31 target |
|
|
142
|
Tuesday, June 24, 2014, 23:57 |
John Wong | SiC | 39530-8 | HP-FEBIAD | In progress | Conditioning SiC#31 target |
|
|
143
|
Wednesday, July 23, 2014, 15:07 |
John Wong | Empty | 40282-3 | LP-SIS | In progress | Sintering TaC coated target container | Wednesday, July 23, 2014, 15:07
Target container is coated with TaC.
No Ta-heat shields are used. |
|
146
|
Tuesday, July 29, 2014, 11:23 |
John Wong | | 40282-3 | LP-SIS | In progress | Sintering ZrC# 6 target |
|
|
151
|
Tuesday, August 05, 2014, 17:20 |
John Wong | | | TARGET BOAT | In progress | Sintering TaC coated end caps |
|
|
152
|
Wednesday, August 06, 2014, 16:10 |
John Wong | Ta | 38817-9 | HP-SIS | In progress | Conditioning Ta target | Wednesday, August 06, 2014, 15:59
Target consists of 400 Ta discs.
Total packed length 4.5cm |
|