Thursday, May 28, 2015, 17:50, John Wong, Endcaps, 40282-5, TARGET BOAT, Done, Sintering TaC coating on Ta endcaps - round 2
|
Laura Lambert wrote:
Thursday, May 28, 2015, 11:34 |
Friday, May 29, 2015, 11:18, Laura Lambert, Endcaps, 40282-5, TARGET BOAT, Done, Sintering TaC coating on Ta endcaps - round 2
|
John Wong wrote:
|
Thursday, May 28, 2015, 10:23, Laura Lambert, Endcaps, 40282-5, TARGET BOAT, Problems, Sintering TaC coating on Ta endcaps - not fully sintered
|
John Wong wrote:
|
Tuesday, May 26, 2015, 13:57, Laura Lambert, Endcaps, 40282-5, TARGET BOAT, In progress, Sintering TaC coating on Ta endcaps
|
Tuesday, May 26, 2015, 13:06
Endcaps were sprayed with TaC coating and let dry.
Each endcap is wrapped separately with a sheet of graphite foil and stacked in the target boat [see image] |
Wednesday, May 27, 2015, 17:58, John Wong, Endcaps, 40282-5, TARGET BOAT, In progress, Sintering TaC coating on Ta endcaps
|
Laura Lambert wrote:
Tuesday, May 26, 2015, 13:06 |
Monday, July 13, 2015, 11:54, Laura Lambert, Endcaps, 40282-5, TARGET BOAT, Problems, Sintering TaC coating on Ta endcaps
|
Monday, July 13, 2015, 11:53
A Ta foil is placed in the target boat with separate slots for each endcap [same as elog 200]
The target boat is wrapped with 3-layers of Ta-heat shield. |
Thursday, August 06, 2015, 15:45, Laura Lambert, Endcaps, , TARGET BOAT, Done, Sintering TaC coating on Ta endcaps
|
Thursday, August 06, 2015, 15:36
The endcaps are stacked together with a punched out disc of graphite foil placed in between each endcap for separation so endcaps won't fuse together.
The end caps are further wrapped in a larger piece of graphite foil to hold together as a tube [same method used in elogID # 158] |
Monday, November 09, 2015, 12:56, John Wong, , 41077-3, LP-SIS, In progress, Sintering TaC coating on 'temporary endcaps' springs (Slope changed to 1.04)
|
Laura Lambert wrote:
Thursday, November 05, 2015, 16:19 |
Monday, November 09, 2015, 14:22, Laura Lambert, , 41077-3, LP-SIS, Done, Sintering TaC coating on 'temporary endcaps' springs (Slope changed to 1.04)
|
John Wong wrote:
|
Thursday, November 05, 2015, 16:20, Laura Lambert, , 41077-3, LP-SIS, In progress, Sintering TaC coating on 'temporary endcaps' springs
|
Thursday, November 05, 2015, 16:19
Springs coated with TaC and loaded into container for sintering.
3x Ta heat shield. |
Tuesday, June 09, 2015, 10:44, Laura Lambert, Empty, 41177-2, LP-SIS, In progress, Sintering TaC coating container for ZrC back-up
|
Tuesday, June 09, 2015, 9:16
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Wednesday, June 10, 2015, 16:35, John Wong, Empty, 41177-2, LP-SIS, In progress, Sintering TaC coating container for ZrC back-up
|
Laura Lambert wrote:
Tuesday, June 09, 2015, 9:16 |
Thursday, June 11, 2015, 16:10, Laura Lambert, Empty, 41177-2, LP-SIS, In progress, Sintering TaC coating container for ZrC back-up
|
John Wong wrote:
|
Tuesday, May 19, 2015, 13:54, Laura Lambert, Empty, 41177-1, LP-SIS, Done, Sintering TaC coating container for ZrC
|
Tuesday, May 19, 2015, 13:33
Target container is coated with TaC. No Ta-heat shields are used.
TGHT will be ramped up to 580A at 0.2A/min. |
Wednesday, May 23, 2018, 15:21, Laura Lambert, Empty, , HP-FEBIAD-CTL, Done, Sintering TaC coating container for UCx#23
|
Wednesday, May 16, 2018, 09:56
Container coated with TaC using 'flushing technique' and let dry over weekend.
Cleaned ionizer tube with acetone, no coating inside ionizer tube. |
Thursday, February 19, 2015, 15:21, Laura Lambert, Empty, 41177-2, LP-SIS, Done, Sintering TaC coating container for UCx#12
|
Thursday, February 19, 2015, 15:19
Target container coated with TaC, loaded in EVAP2.
No Ta heat shields. |
Monday, November 10, 2014, 13:55, Laura Lambert, Empty, , LP-SIS, Done, Sintering TaC coating container for UCx#11 [2nd container]
|
Monday, November 10, 2014, 13:51
target container was sprayed with TaC on friday and sintered over the weekend.
vented and removed from evap2 this morning, looks good. |
Monday, October 06, 2014, 12:17, John Wong, Empty, 40282-5, LP-SIS, In progress, Sintering TaC coating container for UCx#11 (temp measured with OMEGA 2IR)
|
Laura Lambert wrote:
Thursday, October 02, 2014, 11:51 |
Wednesday, October 08, 2014, 11:51, Laura Lambert, Empty, 40282-5, LP-SIS, Done, Sintering TaC coating container for UCx#11 (temp measured with OMEGA 2IR)
|
John Wong wrote:
|
Thursday, October 09, 2014, 16:37, John Wong, Empty, 40282-5, LP-SIS, Done, Sintering TaC coating container for UCx#11 (temp measured with OMEGA 2IR)
|
Laura Lambert wrote:
|
|